The Impact of Hybrid Flame Retardant Compositions on the Performance of Foamed Flexible Polyurethane/Ground Tire Rubber Composites

Authors

[ 1 ] Instytut Technologii Materiałów, Wydział Inżynierii Mechanicznej, Politechnika Poznańska | [ 2 ] Instytut Inżynierii Materiałowej, Wydział Inżynierii Materiałowej i Fizyki Technicznej, Politechnika Poznańska | [ P ] employee

Scientific discipline (Law 2.0)

[2.8] Materials engineering
[2.9] Mechanical engineering
[7.6] Chemical sciences

Year of publication

2024

Published in

Journal of Materials Engineering and Performance

Journal year: 2024 | Journal volume: in press

Article type

scientific article

Publication language

english

Keywords
EN
  • composites
  • flame retardants
  • flammability
  • ground tire rubber
  • polyurethane foams
Abstract

EN Current sustainability-oriented trends affect polyurethane (PU) materials and stimulate the incorporation of recycled or waste-based materials as fillers. Ground tire rubber (GTR) poses as an auspicious candidate due to the excellent performance of car tires. Despite the benefits related to the mechanical performance, it contributes to the increasing flammability of the resulting composites. Herein, presented work assessed the impact of hybrid flame retardant (FR) combinations of ammonium polyphosphate (APP) or melamine cyanurate (MC) with organophosphorus compounds on the performance of foamed flexible PU/GTR composites. Such works are of vital importance, because matching to the needs of material with the mode of action of particular FRs is quite challenging. Except for the flammability reduction, they also affect structure and performance of composites. Fire resistance was enhanced for all applied FRs compositions; however, APP was found more effective than MC due to the efficient formation of protective char layer. Moreover, introduction of MC induced heterogeneity of cellular structure and excessive stiffening of PU structure, which increased its friability and cells coalescence, deteriorating thermal insulation performance and damping ability.

Date of online publication

22.03.2024

DOI

10.1007/s11665-024-09362-1

URL

https://link.springer.com/article/10.1007/s11665-024-09362-1

Ministry points / journal

70

Impact Factor

2,2 [List 2023]

This website uses cookies to remember the authenticated session of the user. For more information, read about Cookies and Privacy Policy.